Dedicated to special alloy product solutions

Inconel MA6000 is a high-temperature alloy composed of elements such as nickel and iron, widely used in aerospace, chemical, and petroleum industries due to its excellent heat resistance and corrosion resistance, making it an important engineering material. Chemical Composition The chemical composition of Inconel MA6000 mainly includes nickel (Ni), iron (Fe), chromium (Cr), molybdenum (Mo), titanium (Ti), cobalt (Co), tungsten (W), and aluminum (Al). Among these, nickel is the primary component, accounting for over 70%. The specific chemical composition is as follows: carbon (C) 0.05%, chromium (Cr) 15%, molybdenum (Mo) 2.0%, titanium (Ti) 2.5%, tungsten (W) 4%, cobalt (Co) 2%, aluminum (Al) 4.5%, with the remainder being nickel.

NS142 is a titanium-stabilized fully austenitic nickel-iron-chromium alloy, with the addition of copper and molybdenum. NS142 is a versatile engineering alloy. It exhibits resistance to corrosion from acids and alkali metals in both oxidizing and reducing environments. The high nickel content provides effective resistance to stress corrosion cracking. Its corrosion resistance is excellent in various media, such as sulfuric acid, phosphoric acid, nitric acid, and organic acids, as well as alkali metals like sodium hydroxide, potassium hydroxide, and hydrochloric acid solutions. The superior overall performance of NS142 is demonstrated in the diverse corrosive media of nuclear fuel dissolution systems, where sulfuric acid, nitric acid, and sodium hydroxide are processed within the same equipment.

MA956 is an ultra-high strength steel, classified as a heat-resistant iron-aluminum-chromium alloy, known for its excellent performance in high-temperature environments. This alloy maintains its stability even under harsh working conditions, making it widely used in various fields such as aerospace, chemical industry, nuclear industry, and marine environments.

Nimonic C263/Nickel Alloy 263 Nickel-based Alloy Chemical Composition: C: ≤0.04–0.08 Cr: 19–21 Ni: balance Mo: 5.6–6.1 W: - Al: 0.3–0.6 Nb: - Ti: 1.9–2.4 Fe: ≤0.70 Si: ≤0.40 Mn: ≤0.60 P: ≤0.015 S: ≤0.007 Co: 19–21 B: ≤0.005 Cu: ≤0.2

Alloy 600 is widely used in the following fields: · Heat exchangers and evaporators in the chemical, pulp, and paper industries · High-temperature components and engine parts in the aerospace field · Catalytic regenerators in petrochemical production · Components in nuclear reactors · Necked bottles and components in heat treatment furnaces, especially in carburizing and nitriding atmospheres.

Alloy C-4 is widely used in the chemical, petroleum, and aerospace industries, particularly suitable for process equipment and piping systems that handle corrosive media such as strong acids, strong oxidizers, and chlorides. Typical application areas include flue gas desulfurization systems, pickling and acid regeneration plants, acetic acid and agricultural chemicals production, titanium dioxide production (chloride process), and electroplating stripping.

Alloy 625 exhibits excellent corrosion resistance in various extreme environments, particularly in seawater, chemicals, and high-temperature corrosive conditions. Its corrosion resistance primarily comes from the synergistic effect of nickel, chromium, and molybdenum, providing strong resistance to oxidation, reduction, pitting, crevice corrosion, and intergranular corrosion. Alloy 625 maintains good mechanical properties at high temperatures (up to 980°C), which gives it high creep and fatigue resistance in high-temperature environments.

Grade 4 is the highest strength among pure titanium grades. It is used in working environments from 0 to 427°C, with intermittent temperatures up to 538°C for welding. The production process involves: releasing pressure at 482-593°C for 30 minutes to 4 hours, followed by air cooling. Annealing is done at 649-816°C for 15 minutes to 2 hours, followed by air cooling. For forgings: closed heating at 871-927°C, completed at 816-871°C.

TA10 titanium is a new type of metal, and the performance of titanium is related to the content of impurities such as carbon, nitrogen, hydrogen, and oxygen. The impurity content of pure titanium iodide does not exceed 0.1%, but it has low strength and high plasticity. The properties of 99.5% industrial pure titanium are: density ρ=4.5g/cm3, melting point 1800℃, thermal conductivity λ=15.24W/(m.K), tensile strength σb=539MPa, elongation δ=25%, reduction of area ψ=25%, elastic modulus E=1.078×105MPa, hardness HB195.

TA9 titanium is a new type of metal, and the performance of titanium is related to the content of impurities such as carbon, nitrogen, hydrogen, and oxygen. The impurity content of pure titanium iodide does not exceed 0.1%, but it has low strength and high plasticity. The properties of 99.5% industrial pure titanium are: density ρ=4.5g/cm3, melting point 1800℃, thermal conductivity λ=15.24W/(m.K), tensile strength σb=539MPa, elongation δ=25%, reduction of area ψ=25%, elastic modulus E=1.078×105MPa, hardness HB195.

TC4 titanium alloy has a series of advantages such as excellent corrosion resistance, low density, high specific strength, and good toughness and weldability. It has been successfully applied in aerospace, petrochemical, shipbuilding, automotive, and medical sectors.

The commonly used industrial pure titanium in industry is TA2, due to its moderate corrosion resistance and comprehensive mechanical properties. When higher wear resistance and strength are required, TA3 can be used. For better forming properties, TA1 can be used.

Titanium is a new type of metal, and its properties are related to the content of impurities such as carbon, nitrogen, hydrogen, and oxygen. Pure titanium iodide has an impurity content of no more than 0.1%, but it has low strength and high plasticity. The properties of 99.5% industrial pure titanium are: density ρ = 4.5 g/cm³, melting point 1800°C, thermal conductivity λ = 15.24 W/(m·K), tensile strength σb = 539 MPa, elongation δ = 25%, reduction of area ψ = 25%, elastic modulus E = 1.078 × 10^5 MPa, hardness HB195.