GH2036 (GH36) high-temperature alloy
GH2036 (GH36) high-temperature alloy is a type of iron-based high-temperature alloy that is age-hardened and composed of elements such as chromium, molybdenum, and nickel, with a nickel content of about 8%. GH2036 (GH36) high-temperature alloy has good hot and cold working properties, a simple alloy composition, stable microstructure, and exhibits good physical and mechanical properties at 600-650°C, along with excellent machinability. The alloy has a large coefficient of expansion.
Classification:
Key words:
Superalloy | Inkenel | Hastelloy | Inkloy | Precision Alloy Series
Product Parameters
GH2036
Material grade: GH2036 (GH36) high-temperature alloy
1.Overview of GH2036 (GH36) high-temperature alloy:
GH2036 (GH36) high-temperature alloy is a type of age-hardened iron-based high-temperature alloy composed of elements such as chromium, molybdenum, and nickel, with a nickel content of about 8%. GH2036 (GH36) high-temperature alloy has good hot and cold working properties, simple alloy composition, stable structure, and exhibits good physical and mechanical properties at 600-650℃, along with good machinability, and a large coefficient of thermal expansion.
2.Chemical composition of GH2036 (GH36) high-temperature alloy:See Table-1:
Table-1
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.34-0.40 | 0.30-0.80 | 7.50-9.50 | 0.035 | 0.030 | 11.5-13.5 | 7.0-9.0 | 1.10-1.40 | |
| Others | N≤ | Al≤ | Ti≤ | Fe≤ | Co≤ | V≤ | W≤ | Nb≤ |
| - | 0.12 | Remainder | 1.25-1.55 | 0.25-0.55 |
3.Mechanical properties of GH2036 (GH36) high-temperature alloy:
1. Tensile strength σb (MPa): ≥850
2. Yield strength σ0.2 (MPa): 600
3. Elongation δ5 (%): ≥15
4. Reduction of area ψ (%): ≥20
5. Hardness (HB)/mm (compression d): 3.45-3.65
6. Heat treatment process: Solution: 1140±5℃, hold for 80 min for diameter less than 45mm. Hold for 105 min for diameter not less than 45mm, then cool in flowing water. Aging: Place in a furnace below 670℃, hold for 12-14h, then raise to 770-800℃, hold for 12-14h, air cool.
7. Metallographic structure: Age-hardened iron-based alloy
4.Characteristics and applications of GH2036 (GH36) high-temperature alloy:
1. GH2036 (GH36) high-temperature alloy is an austenitic alloy steel, which has high strength below 650℃ and good hot working and machining properties. It has stable oxidation resistance in air media at 700-750℃, but tends to intergranular corrosion in gas media at 700-750℃ and higher temperatures. The alloy has a large coefficient of thermal expansion, and it has been found that GH2036 discs are prone to defects such as large grains and cracks during production and use, and new alloys are being researched to replace it.
2. Applications of GH2036 (GH36) high-temperature alloy: Used for turbine discs, thermal insulation plates, protective rings, load-bearing ring fasteners, etc., working below 650℃.
5.Varieties, specifications, and supply status of GH2036 (GH36) high-temperature alloy:
1. Variety classification: Seamless pipes, welded pipes, plates, bars, forgings, rings, wires, and matching welding materials.
2. Delivery status: Seamless pipes: solution + acid pickling, length can be customized; plates: solution, acid washing, edge cutting; welded pipes: solution acid pickling + RT% flaw detection, forgings: annealed + turned; bars in forged state, surface polished or turned; strips delivered after cold rolling, solution soft state, and descaling; wires delivered in solution acid-washed coil or straight bar form, solution straight bar finely polished.