GH1140/GH140 high-temperature alloy
GH1140 high-temperature alloy is a solid solution strengthened iron-nickel-based high-temperature alloy. In addition to containing a large amount of chromium, it is also reinforced with a small amount of tungsten, molybdenum, aluminum, and titanium. The alloy has moderate thermal strength, high plasticity, good thermal fatigue resistance, structural stability, and welding process performance. It is suitable for manufacturing sheet structural components and other high-temperature parts for aircraft engines and gas turbine combustion chambers operating at temperatures below 850°C. Various deformed products such as plates, rods, pipes, wires, strips, and forgings can be supplied.
Classification:
Key words:
Superalloy | Inkenel | Hastelloy | Inkloy | Precision Alloy Series
Product Parameters
GH1140
Chinese grade: GH1140/GH140 high-temperature alloy
1.Overview of GH1140 high-temperature alloy:
GH1140 high-temperature alloy is a solid solution strengthened iron-nickel-based high-temperature alloy, which contains a large amount of chromium and is compounded with a small amount of tungsten, molybdenum, aluminum, and titanium to enhance the solid solution. The alloy has moderate thermal strength, high plasticity, good thermal fatigue resistance, structural stability, and welding process performance. It is suitable for manufacturing structural components and other high-temperature parts for aircraft engines and gas turbine combustion chambers with operating temperatures below 850°C. Various deformed products such as plates, rods, pipes, wires, strips, and forgings can be supplied.
1. GH1140 material grade: GH1140 (GH140, CR-2).
2. Technical standards for GH1140 material:
GJB 1952-1994 "Specification for Cold-Rolled Thin Plates of High-Temperature Alloys for Aviation"
GJB 2297-1995 "Specification for Cold-Drawn (Rolled) Seamless Pipes of High-Temperature Alloys for Aviation"
GJB 2612-1996 "Specification for Cold-Drawn Wire of High-Temperature Alloys for Aviation"
GJB 3020-1997 "Specification for Ring Blanks of High-Temperature Alloys for Aviation"
GJB 3317-1998 "Specification for Hot-Rolled Plates of High-Temperature Alloys for Aviation"
GJB 3318-1998 "Specification for Cold-Rolled Strips of High-Temperature Alloys for Aviation"
GJB 3165-1998 "Specification for Hot-Rolled and Forged Bars of High-Temperature Alloys for Aviation Load-Bearing Parts"
GJB 3167-1998 "Specification for Cold-Drawn Wire of High-Temperature Alloys for Cold Heading"
3. Chemical composition of GH1140: see Table 1-1:
Table 1-1
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.06-0.12 | 0.80 | 0.70 | 0.025 | 0.015 | 20.0-23.0 | 35.0-40.0 | 2.00-2.50 | |
| Others | N≤ | Al≤ | Ti≤ | Fe≤ | Ce≤ | V≤ | W≤ | Nb≤ |
| 0.20-0.60 | 0.70-1.20 | Remaining | 0.05 | 1.40-1.80 |
Note: When smelting with an electric arc furnace, ω(Al+Ti) should not exceed 1.55%, and when using electric arc furnace + electroslag remelting, ω(Al+Ti) should not exceed 1.75%.
4. Heat treatment system for GH1140: Solution treatment: Hot-rolled plates, cold-rolled thin plates, and strips at 1050~1090℃, air-cooled; wire and pipe at 1050~1080℃, air-cooled or water-cooled; bars and ring blanks at 1080℃±10℃, air-cooled.
5. Variety specifications and supply status: Various specifications of hot-rolled plates, cold-rolled plates, strips, bars, wires, pipes, forgings, and ring parts can be supplied. Plates, pipes, wires, and strips are supplied after solution treatment and pickling. Bars and ring parts are supplied in hot-rolled or forged state. Forgings are supplied in forged state or after solution treatment.
6. Smelting and casting process: Electric arc furnace melting or electric arc furnace + electroslag remelting.
7. Application overview and special requirements: It has been used to manufacture various components such as combustion chamber flame tubes, afterburner diffusers, rectifier support plates, stabilizers, oil delivery rings, adjustable nozzle housings, pipe joints, bushings, and aircraft tail cover skins, and has been put into batch production. After long-term use in the temperature range of 550~800℃, slight hardening occurs, reducing room temperature plasticity. Its high-temperature oxidation resistance above 1000℃ is slightly worse than that of nickel-based alloys for similar applications.
2.Physical and chemical properties of GH1140 high-temperature alloy:
1. Physical properties:
(1) Density: ρ=8.09g/cm3
(2) Electrical properties: Room temperature resistivity ρ=1.07*10-6Ω.m
(3) Magnetic properties: The alloy is non-magnetic.
2. Chemical properties:
(1) Oxidation resistance:
a. The oxidation rate of the alloy tested in air medium for 100 hours.
b. The alloy produces intergranular oxidation during long-term work above 700℃. The maximum intergranular oxidation depth after exposure for 100 hours at 700℃~1200℃. The maximum intergranular oxidation depth after long-term exposure for 1000 hours at 700~900℃.
c. The flame tubes made of this alloy may experience oxidation spalling during long-term work above 900℃; the spalling rate is 0.016mm/100h. The oxidation spalling depth in the middle section of the flame tube after long-term work.
d. Alloys can be effectively protected with enamel coatings such as 65, 66-4, W-2, and W69-1 when working at high temperatures for a long time, or by using solid aluminum diffusion and vacuum aluminum plating.
(2) Corrosion resistance: Domestic aviation kerosene has no corrosive effect on GH1140 alloy, whether or not CS2 additives are present, while nickel-based alloys require additives to prevent corrosion. When using foreign aviation kerosene, severe pitting corrosion is sometimes observed.
Three,GH1140 high-temperature alloy hot forming process:
1. Hot forming process:
(1) The furnace temperature during forging should be ≤700℃, heating temperature 1160℃±20℃, and the final temperature should not be lower than 900℃.
(2) The heating temperature for hot rolling of slabs is 1160℃±20℃, rolling temperature is 1180~950℃, and the temperature should preferably be controlled in the range of 950~1000℃ when entering the last pass.
(3) The heating temperature for hot-rolled plates is 1120℃, rough rolling temperature is 1120~850℃, and the total deformation amount for the first hot rolling of hot-rolled plates should be greater than 50%.
(4) The reduction amount for cold-rolled plates is 30%~40%, and the flatness deformation amount of the finished plate should not exceed 3%.
2. Cold forming performance: The state of the plate has good plasticity, and the forming process is carried out at room temperature. When manufacturing parts using multiple forming processes, intermediate heat treatment is performed after each cold forming. The surface of the parts is coated with nitro varnish before forming.
Four,Varieties, specifications, and supply status of GH1140 high-temperature alloy:
1. Variety classification: seamless pipes, welded pipes, plates, bars, forgings, rings, wires, and matching welding materials.
2. Delivery status: Seamless pipes: solution + acid pickling, length can be customized; plates: solution, acid washing, edge cutting; welded pipes: solution acid pickling + RT% flaw detection, forgings: annealing + turning; bars in forged and rolled state, surface polished or turned; strips delivered in cold-rolled, solution soft state, and descaled; wires delivered in solution acid-washed coil or straight bar form, solution straight bar finely polished state.