Product classification
GH1040 iron-based high-temperature alloy
GH1040 iron-based high-temperature alloy is a solid solution strengthened iron-based high-temperature alloy composed of elements such as nickel, molybdenum, chromium, and nitrogen, with a nickel content of about 26%. The GH1040 high-temperature alloy has good hot and cold working properties, and can achieve sufficiently high instantaneous strength for short-term use at temperatures between 990-1000°C; it also has good plasticity during hot processing.
Classification:
Key words:
Superalloy | Inkenel | Hastelloy | Inkloy | Precision Alloy Series
Product Parameters
GH1040
Chinese grade: GH1040 iron-based high-temperature alloy
Material grade: GH1040
1.Overview of GH1040 iron-based high-temperature alloy:
GH1040 iron-based high-temperature alloy is a solid solution strengthened iron-based high-temperature alloy composed of elements such as nickel, molybdenum, chromium, and nitrogen, with a nickel content of about 26%. GH1040 high-temperature alloy has good thermal and cold processing performance, and can achieve sufficiently high instantaneous strength for short-term use at 990-1000℃; it has good hot processing plasticity.
2.Chemical composition of GH1040 iron-based high-temperature alloy:See Table-1.
Table-1
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.12 | 0.50-1.000 | 1.00-2.00 | 0.030 | 0.020 | 15.0-17.5 | 24.0-27.0 | 5.5-7.00 | - |
| Others | B≤ | Ce≤ | N≤ | Fe≤ | Co≤ | V≤ | W≤ | Nb≤ |
| - | - | 0.10-0.20 | Remaining | - | - | - | - |
3.Applications of GH1016 high-temperature alloy:
GH1016 is suitable for service temperatures of 550-1000℃, used for manufacturing general load-bearing components in aerospace, aviation, gas turbines, and other industries (excluding turbine blades), and for components such as combustion chambers and afterburner chambers in turbine engines working below 950℃.
4.Physical properties of GH1040 high-temperature alloy:
1. GH1040 tensile strength σb (MPa): ≥520
2. GH1040 yield strength σ0.2 (MPa): ≥205 elongation δ5 (%): ≥40
3. GH1040 reduction of area ψ (%): ≥50
4. GH1040 hardness: ≤187HB; ≤90HRB; ≤200HV
5.Heat treatment specifications and metallographic structure of GH1040 high-temperature alloy:
1. Heat treatment specifications: solution treatment at 1010-1150℃ with rapid cooling.
2. Metallographic structure: characterized by austenitic structure.
6.Delivery condition of GH1040 high-temperature alloy:
Generally delivered in heat-treated condition, with the type of heat treatment specified in the contract; if not specified, delivered in non-heat-treated condition.
7.Varieties, specifications, and supply conditions of GH1040 high-temperature alloy:
1. Variety classification: seamless pipes, welded pipes, plates, bars, forgings, rings, wires, and matching welding materials.
2. Delivery condition: seamless pipes: solution + acid pickling, length can be specified; plates: solution, acid washing, edge cutting; welded pipes: solution acid pickling + RT% flaw detection, forgings: annealed + turned; bars in forged state, surface polished or turned; strips delivered after cold rolling, solution soft state, and descaling; wires delivered in solution acid washed coil or straight bar form, solution straight bar finely polished.