Product classification
GH2132
Nickel-based alloy GH2132 (GH132) is a precipitation-hardened, deformed high-temperature alloy, primarily composed of iron, nickel, and chromium, with the addition of molybdenum, titanium, aluminum, vanadium, and trace amounts of boron for comprehensive strengthening. This alloy exhibits high yield strength and long-term creep strength below 650°C, while also demonstrating good machinability and satisfactory welding performance.
Classification:
Key words:
Superalloy | Inkenel | Hastelloy | Inkloy | Precision Alloy Series
Product Parameters
1. Overview
Nickel-based alloy GH2132 (GH132) is a precipitation-hardened, deformed high-temperature alloy, primarily composed of iron, nickel, and chromium, with the addition of molybdenum, titanium, aluminum, vanadium, and trace boron for comprehensive strengthening. This alloy exhibits high yield strength and long-term creep strength below 650°C, while also demonstrating good processing plasticity and satisfactory welding performance.
2. Chemical Composition
The chemical composition of GH2132 alloy mainly includes: Carbon (C) ≤ 0.08%, Chromium (Cr) 13.5~16.0%, Nickel (Ni) 24.0~27.0%, Molybdenum (Mo) 1.00~1.50%, Titanium (Ti) 1.90~2.30% (with cold drawn bars, discs, and ring blanks specified as 1.80%~2.35%), with the remainder being iron (Fe). Additionally, it contains certain amounts of vanadium (V), boron (B), manganese (Mn), aluminum (Al), silicon (Si), phosphorus (P), and sulfur (S) to meet its comprehensive performance requirements.
3. Physical and Chemical Properties
Thermal properties: The melting temperature range of GH2132 alloy is 1364~1424°C. Its thermal conductivity increases with temperature, for example, at 100°C the thermal conductivity is 14.2 W/(m·°C), and at 900°C it increases to 23.9 W/(m·°C).
Linear expansion coefficient: The linear expansion coefficient of this alloy increases with temperature, for example, in the range of 20~100°C it is 15.37×10^-6/°C, and in the range of 20~900°C it increases to 20.45×10^-6/°C.
Density: The density of GH2132 alloy is 7.93 g/cm³.
Resistivity: Its resistivity increases with temperature, for example, at 20°C it is 0.914×10^-6 Ω·m, and at 900°C it increases to 1.135×10^-6 Ω·m.
Chemical properties: After testing in air for 100~300 hours, the oxidation rate of GH2132 alloy is relatively low, for example, at 650°C after 100 hours, the oxidation rate is 0.00417 g/(m²·h).
4. Application Fields
Due to its excellent high-temperature performance, GH2132 alloy is widely used in the following fields:
Aerospace engines: Manufacturing high-temperature load-bearing components for aerospace engines that operate long-term below 650°C, such as turbine discs, compressor discs, rotor blades, and fasteners.
Industrial gas turbines: Manufacturing components and various fasteners for industrial gas turbines.
Automotive engines: Also widely used in automotive engines.
Other high-temperature environments: Suitable for other applications requiring high temperature and high strength, such as reactors, heat exchangers, and storage tanks in nuclear reactors, chemical, and petrochemical industries.
5. Heat Treatment Process
The heat treatment process of GH2132 alloy has a significant impact on its performance, mainly including the following steps:
Material selection and inspection: Select high-quality nickel-based alloy raw materials and conduct strict inspections.
Surface treatment: Perform peeling, rust removal, and polishing on raw materials to remove impurities and oxides.
Melting: Use a vacuum induction furnace for melting, strictly controlling melting parameters to ensure the uniformity and purity of the alloy composition. During the melting process, appropriate amounts of trace elements are added to enhance the performance of the alloy.
Forging: Forge the melted alloy ingot to make its structure denser and more uniform. Strictly control the degree of deformation and temperature during the forging process to avoid overheating and overload.
Annealing: To eliminate forging stress and improve the plasticity and toughness of the alloy, annealing treatment is performed. During the annealing process, control the temperature, holding time, and cooling rate to achieve the desired microstructure.
Machining: The alloy after annealing can undergo subsequent machining.
Final heat treatment: Conduct final heat treatment according to the operating environment and performance requirements of the parts. Common methods include quenching and tempering, aging, surface hardening, etc. Strictly control temperature, holding time, and cooling rate to achieve optimal performance.
In addition, the strength and creep resistance of GH2132 alloy can be further improved through solution treatment and aging treatment. The solution treatment temperature is generally controlled between 1050°C and 1100°C, with a holding time of 2 to 4 hours, followed by rapid cooling; the aging treatment temperature is controlled between 700°C and 750°C, with a holding time of 16 to 24 hours.
6. Conclusion
GH2132 (GH132) nickel-based alloy, with its excellent high-temperature performance, good processing plasticity, and satisfactory welding performance, has become an ideal choice for high-temperature environments such as aerospace, gas turbines, and nuclear reactors. Through reasonable heat treatment operations, its performance can be further enhanced to meet various application needs in high-temperature environments.