GH4037/GH37 high-temperature alloy
GH3037 (GH37) alloy is an austenitic age-hardened nickel-based alloy, with a total addition of about 4% aluminum and titanium to form the γ phase for age hardening. It also contains a significant amount of tungsten and molybdenum for solid solution strengthening, and a trace amount of boron to strengthen the grain boundaries. This alloy is used below 850°C, exhibiting high thermal strength, good overall performance, and structural stability, and is widely used in the manufacture of turbine blades for aircraft engines, with long-term use at temperatures between 800-850°C.
Classification:
Key words:
Superalloy | Inkenel | Hastelloy | Inkloy | Precision Alloy Series
Product Parameters
GH4037
Chinese grade: GH4037/GH37 high-temperature alloy
Foreign grade: Зи617 XH70BMTTЮ (Russia)
1.Overview of GH4037 high-temperature alloy:
GH3037 (GH37) alloy is an austenitic age-hardened nickel-based alloy, with a total addition of about 4% aluminum and titanium to form the γ phase for age hardening, and a significant amount of tungsten and molybdenum for solid solution strengthening, along with trace amounts of boron to strengthen the grain boundaries. This alloy is used below 850°C, exhibiting high thermal strength, good comprehensive performance, and structural stability, widely used in the manufacture of turbine working blades for aircraft engines, with long-term use below 800-850°C.
1. Characteristics of GH4037 high-temperature alloy:
(1) GH4037 (GH37): Easy to process.
(2) GH4037 (GH37): High thermal strength, good comprehensive performance, and structural stability at 850°C.
(3) GH4037 (GH37): High oxidation resistance and long-term structural stability at 850°C.
(4) GH4037 (GH37): Suitable for long-term use of turbine working blades for aircraft engines below 800~850°C.
(5) GH4037 (GH37): Good welding performance.
2. Application fields of GH4037 high-temperature alloy: Due to its moderate thermal strength and good thermal fatigue performance below 850°C, it can be widely applied in various high-demand situations, such as aircraft engines, combustion chambers, afterburner components, acidic environments, and turbine working blades.
3. Standards for GH4037 high-temperature alloy:
(1) GB/T 14992-2005 "Standard for High-Temperature Alloy Grades."
(2) GB/T14993-1994 "Hot-Rolled Bars of High-Temperature Alloys for Rotating Parts."
(3) GB/T14994-1994 "Cold-Drawn Bars of High-Temperature Alloys."
(4) GB/T14995-1994 "Hot-Rolled Plates of High-Temperature Alloys."
(5) GB/T14996-1994 "Cold-Rolled Thin Plates of High-Temperature Alloys."
(6) GB/T14996-1994 "Cold-Rolled Thin Plates of High-Temperature Alloys."
4. Chemical composition of GH4037 high-temperature alloy: See Table-1:
Table-1 %
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.03-0.10 | 0.40 | 0.50 | 0.015 | 0.010 | 13.0-16.0 | Remainder | 2.0-4.0 | - |
| Others | N≤ | Al≤ | Ti≤ | Fe≤ | B≤ | Ce≤ | W≤ | Nb≤ |
| - | 1.70-2.30 | 1.80-2.30 | 5.00 | 0.02- | 0.02 | 5.0-7.0 | - |
2.Physical properties of GH4037 high-temperature alloy:
1. Density of GH4037 high-temperature alloy: ρ=8.4g/cm3.
2. Melting temperature range of GH4037 high-temperature alloy: 1278~1346°C.
3. Metallographic structure of GH4037 high-temperature alloy: The structure of this alloy in the standard heat-treated state consists of an austenitic matrix and dispersed γ phase, with a small amount of M23C6 and M6C type carbides at the grain boundaries, and blocky MC type carbides within the grains.
3.Process performance and requirements of GH4037 high-temperature alloy:
1. This alloy has good forgeability, with forging heating temperature at 1140°C and final forging at 1100°C.
2. The average grain size of this alloy is closely related to the degree of deformation of the forged piece and the final forging temperature.
3. During heat treatment of the blades, slow heating is required, using a step heating curve to reach the solution temperature, with strict temperature control. To ensure the stability of the blade performance, special attention should be paid to the cooling rate during secondary solution treatment, which should not be too fast.
4. After mechanical processing of the blades, if necessary, to eliminate residual stress in the surface layer, the finished parts should undergo stress relief tempering, with the specification as follows: heat in argon at 950°C for 2 hours, cool to 700°C in the heating box, then air cool. After that, heat at 800°C for 8 hours, then air cool. After this treatment, not only can the residual stress on the blade surface be eliminated, but also the notch sensitivity can be improved.
4.Varieties, specifications, and supply status of GH4037 high-temperature alloy:
1. Variety classification: GH4037 seamless pipes, GH4037 welded pipes, GH4037 plates, GH4037 bars, GH4037 forgings, GH4037 rings, GH4037 wires, and matching welding materials.
2. Delivery Status: Seamless pipe: solution + acid pickling, length can be customized; plate: solution, acid washing, edge cutting; welded pipe: solution acid pickling + RT% flaw detection, forgings: annealed + turned; bar material in forged and rolled state, surface polished or turned; strip material delivered after cold rolling, solution soft state, and descaling; wire material delivered in solution acid washed coil or straight bar form, solution straight bar fine polished state.