Product classification
GH738 high-temperature alloy
GH738 is a nickel-based superalloy that is precipitation-hardened with the γ′ phase. It has good resistance to gas corrosion, high yield strength, and fatigue performance, along with good process plasticity and stable microstructure. It is widely used in rotating components of aircraft engines, with a service temperature not exceeding 815°C. It can be produced in cold-rolled and hot-rolled sheets, pipes, strips, wires, as well as forgings, castings, and fasteners.
Classification:
Key words:
Superalloy | Inkenel | Hastelloy | Inkloy | Precision Alloy Series
Product Parameters
GH738
Chinese grade: GH738 nickel-based high-temperature alloy
American grade: Waspaloy
French grade: NC20K14
1.Overview of GH738 nickel-based high-temperature alloy:
GH738 is a nickel-based high-temperature alloy that is precipitation hardened with the γ′ phase, featuring good resistance to gas corrosion, high yield strength, and fatigue performance, along with good process plasticity and stable microstructure. It is widely used in rotating parts of aircraft engines, with a maximum service temperature of 815℃. It can be produced in cold-rolled and hot-rolled plates, pipes, strips, wires, forgings, castings, and fasteners.
1. GH738 material grade: GH738
2. Similar grades to GH738: Waspaloy (USA), NC20K14 (France)
3. Technical standards for GH738 material:
4. Chemical composition of GH738: See Table 1-1.
Table 1-1 %
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.03-0.10 | 0.15 | 0.10 | 0.015 | 0.015 | 18.0-21.0 | Remainder | 3.5-5.0 | 0.10 |
| Others | N≤ | Al≤ | Ti≤ | Fe≤ | Co≤ | B≤ | Zr≤ | Nb≤ |
| - | 1.20-1.60 | 2.75-3.25 | 2.00 | 12.0-15.0 | 0.003-0.01 | 0.02-0.08 | - |
Note: Trace impurities are ω(Pb)≤0.001%, ω(As)≤0.0025%, ω(Sn)≤0.0012%, ω(Sb)≤0.0025%, ω(Bi)≤0.0001%.
5. GH738 heat treatment process: 1080℃±10℃, 4h, air cooling + 840℃, 24h, air cooling + 760℃, 16h, air cooling.
6. Specifications and supply status of GH738: Can produce bars, profiles, forgings, rings, thick plates, thin plates, strips, pipes, wires, sand castings, precision castings, and fasteners, usually delivered without heat treatment; plates are delivered after solution treatment.
7. GH738 melting and casting process: Uses vacuum induction melting combined with vacuum arc remelting.
8. Overview of GH738 applications and special requirements: This alloy is widely used abroad in aircraft engines and gas turbines, mainly as rotating parts such as turbine blades and discs, with mature usage experience. Due to the high cobalt content of this alloy, it is less commonly used domestically.
2.Physical and chemical properties of GH738:
1. Thermal properties of GH738:
(1) Melting temperature range of GH738: 1330~1360℃.
(2) Thermal conductivity of GH738: See Table 2-1.
Table 2-1[1]
| θ/℃ | 360 | 460 | 545 | 640 | 770 | 855 | 985 |
| λ/(W/(m·℃)) | 16.8 | 18.3 | 20.2 | 22.4 | 24.1 | 25.3 | 28.0 |
(3) Specific heat capacity of GH738: See Table 2-2.
Table 2-2[1]
| θ/℃ | 360 | 460 | 545 | 640 | 770 | 855 | 985 |
| c/(J/(kg.℃)) | 515 | 540 | 573 | 603 | 640 | 665 | 707 |
(4) Linear expansion coefficient of GH738: See Table 2-3.
Table 2-3[1]
| θ/℃ | 20-100 | 20-200 | 20-300 | 20-400 | 20-500 | 20-600 | 20-700 | 20-800 | 20-900 |
| α/10-6℃-1 | 12.47 | 12.73 | 13.04 | 13.53 | 13.97 | 14.47 | 15.05 | 15.68 | 15.95 |
2. Density of GH738: ρ=8.22g/cm.3.
3. Electrical properties of GH738:
4. Magnetic properties of GH738: The alloy is non-magnetic.
5. Chemical properties of GH738:
(1) Oxidation resistance of GH738: The oxidation rate of the alloy after 100 hours of testing in air is shown in Table 2-4.
(2) Corrosion resistance of GH738: The alloy has good resistance to salt spray corrosion.
Table 2-4[1]
| θ/℃ | 900 | 1000 |
| Oxidation rate/(g/(m2)· h)) | 0.083 | 0.226 |
Three,Mechanical properties of GH738: The performance specified by the GH738 technical standard: see Table 3-1.
Table 3-1
| Tensile properties | HBS | Durability | ||||||
| θ/℃ | σb/MPa | δ5/% | φ/% | θ/℃ | σ/MPa | t/h | δ5/% | |
| Not less than | Not less than | |||||||
| 815 | 608 | 20 | 32 | 299~387 | 815 | 328 | 23 | 8 |
Four,Microstructure of GH738:
1. GH738 phase transformation temperature: The dissolution temperature of the γ′ phase in the alloy is 980~1050℃, the temperature at which it begins to precipitate from the matrix is 630℃, and the peak precipitation temperature is 800℃. The starting precipitation temperature of the MC carbide phase in the alloy is 700℃, and the complete dissolution temperature is 1020℃.23C62. GH738 time-temperature-structure transformation curve:
3. GH738 alloy microstructure:
After standard heat treatment, except for the austenite matrix, this alloy was aged at 650℃ and 730℃ for up to 3000h, with no significant change in the quantity of the γ′ phase, with approximately 3% and 1% supplementary precipitation, respectively, and the size of the γ′ phase grew from 146nm to 196nm and 177nm. The MC carbide transformed to M.
The total amount of carbide slightly increased, from 0.5% of the total matrix before aging to 0.76% and 0.78%. No new phases precipitated during the long-term aging process, and the structure remained stable.23C6Five,
Process performance and requirements of GH738:1. Formability of GH738:
(1) The plasticity diagram of GH738 alloy is shown in Figure 5-1.
(2) The recrystallization diagram of GH738 alloy is shown in Figure 5-2.
(3) The GH738 alloy has good hot working plasticity and is a relatively well-formable nickel-based high-temperature alloy. The forging billet heating temperature is 1150~1170℃, the suitable hot working temperature is 1040~1170℃, and the final forging temperature should not be lower than 1000℃. The forging temperature for turbine blades is usually in the range of 1070~1110℃, and the minimum deformation amount for die forging should be greater than 25%. It is advisable to avoid hot working with small deformation amounts (about 10%) at high temperatures (1180℃), as this may lead to the formation of continuous MC-type carbide films at the grain boundaries, resulting in notch sensitivity. At lower temperatures (980~1080℃), hot deformation rarely forms MC carbide films at the grain boundaries, only discontinuous M-type carbides, and a uniform grain size of 4~5 levels can be obtained after heat treatment, with good overall performance.
2. Heat treatment process for GH738 parts: During the heat treatment of parts, care should be taken to prevent element depletion on the surface of the parts, and heating should be uniform.23C63. Surface treatment process for GH738: When this alloy is used for rotating parts such as turbine blades and turbine discs, in order to improve fatigue performance, argon gas protection stress relief annealing and shot peening treatment should be performed. To enhance the resistance of turbine blades to gas corrosion and thermal fatigue, diffusion aluminizing treatment can be carried out.
Six,
Varieties, specifications, and supply status of GH738:
1. Variety classification: GH738 seamless pipes, GH738 steel plates, GH738 round steel, GH738 forgings, GH738 flanges, GH738 rings, GH738 welded pipes, GH738 steel strips, GH738 wires, and GH738 matching welding materials.2. Delivery status: Seamless pipes: solution + acid pickling, length can be customized; plates: solution, acid washing, edge cutting; welded pipes: solution acid pickling + RT% flaw detection, forgings: annealing + turning; bars in forged state, surface polished or turned; strips delivered after cold rolling, solution soft state, and descaling; wires delivered in solution acid-washed coil or straight bar form, solution straight bar fine polished state.
1、品种分类:GH738无缝管、GH738钢板、GH738圆钢、GH738锻件、GH738法兰、GH738圆环、GH738焊管、GH738钢带、GH738丝材及GH738配套焊材。
2、交货状态:无缝管:固溶+酸白,长度可定尺;板材:固溶、酸洗、切边;焊管:固溶酸白+RT%探伤,锻件:退火+车光;棒材以锻轧状态、表面磨光或车光;带材经冷轧、固溶软态、去氧化皮交货;丝材以固溶酸洗盘状或直条状、固溶直条细磨光状态交货。