Product classification
GH39
GH39 high-temperature alloy detailed explanation: This alloy is a single-phase austenitic solid solution strengthened alloy, which has moderate thermal strength and good thermal fatigue performance below 800°C. It has good oxidation resistance below 1000°C, stable microstructure for long-term use, and also possesses good cold formability and weldability. It is suitable for long-term use in aircraft engine combustion chambers and afterburner components below 850°C.
Classification:
Key words:
Superalloy | Inkenel | Hastelloy | Inkloy | Precision Alloy Series
Product Parameters
GH39 High-Temperature Alloy Details:
This alloy is a single-phase austenitic solid solution strengthened alloy, which has moderate thermal strength and good thermal fatigue performance below 800℃, good oxidation resistance below 1000℃, stable microstructure for long-term use, and also has good cold formability and welding performance. It is suitable for components in aircraft engine combustion chambers and afterburner chambers for long-term use below 850℃.
GH39 High-Temperature Alloy Chemical Composition:
Carbon C (≤0.08)
Chromium Cr (19.0~22.0)
Nickel Ni (balance)
Molybdenum Mo (1.80~2.30)
Titanium Ti (0.35~0.75)
Niobium Nb (0.90~1.30)
Iron Fe (not more than 3.0)
Manganese Mn (not more than 0.40)
Aluminum Al (0.35~0.75)
Silicon Si (not more than 0.80)
Phosphorus P (not more than 0.020)
Sulfur S (not more than 0.012)
Technical Standards: GB/T14992, GB/T14993
GH39 Physical Properties Description:
Density: 8.3g/cm3
GH39 Mechanical Properties Description:
Variety |
Heat Treatment Method |
Tensile Strength |
Yield Strength |
Elongation |
Reduction of Area Ψ/% |
Brinell Hardness HBS |
Cold Rolled Plate |
Solution + Aging |
735 |
--- |
40 |
--- |
--- |
Bar Stock |
Solution + Aging |
735 |
--- |
40 |
--- |
--- |
GH39 Processing Technology Description:
GH39 Melting Process:
Electric arc melting, electric arc furnace or non-vacuum induction furnace + electroslag remelting or vacuum electric arc remelting, as well as vacuum induction furnace + electroslag or vacuum electric arc remelting process.
GH39 Forging Process:
GH39 alloy has good deformation performance, forging heating temperature is 1170~1190℃, final forging temperature not lower than 900℃, and the deformation amount for one heating is 50%.
GH39 Parts Heat Treatment Process:
The intermediate solid solution heat treatment temperature for parts is 1050℃, air-cooled; the final heat treatment temperature for combustion chamber parts is 1080℃, air-cooled. For parts requiring high durability, the solid solution temperature can be increased to 1170℃. The holding time during solid solution heat treatment can be selected based on thickness, ranging from 5 to 20 minutes.